Al₂O₃: | ≥40% | Density: | 0.6-1.0/cm³ |
---|---|---|---|
Shape: | Customized | Size: | Customized |
Customized Fire Clay Insulating Bricks Lightweght Bricks Henan Clay Brick Factory
In light weight fire clay brick, Al₂O₃ is more than 40%, Fe2O3 is less than 2.0~2.5%. In its ingredient, clinker is 65~85%, binding clay is 10~30%. We manufacture it by mixed grinding the crushed combined clay and levigated clinker, confecting with particle clinker into medium dry pug, high pressure molding, firing under the temperature of 1400℃ with good performance.
Physical and Chemical Index:
Index |
Light Weight Fire Clay Brick | ||
QN-0.6 | QN-0.8 | QN-1.0 | |
Bulk & Density (g/cm3) ≥ | 0.6 | 0.8 | 1.0 |
Cold Crushing Strength (MPa) ≥ | 2.0 | 3.0 | 4.0 |
Heat Conductivity (900℃±25) (W/m·k) ≤ | 0.25 | 0.30 | 0.50 |
Project cases:
Applications:
Light weight fire clay brick is of low price, but of good thermal vibration stability and thermal insulation, mainly used in thermal boiler, glass kiln, cement kiln, fertilizer gas furnace, blast furnace, hot-blast stove, coking furnace, electric furnace, casting, etc.
Welcome you to our factory:
Packing: